I have an agitated vessel that we inject live steam into for direct heating/mixing. The vessel is 8 y/o. The welds at the support lugs have developed leaks due to cracks. The shell is Incoloy 800 and the support lugs, which distribute the stresses, are SA-285 carbon steel. I'm looking to replace it with a new one.
Questions
1) Would PWHT the vessel prevent this???
2) Could/should I specfiy the lugs be Alloy 800???
3) The lugs are attached to the vessel with a SA-285 pad. I'm thinking if I change the Pad to Alloy 800, the dissimilar weld will be moved off the pressure retaining shell.
Thoughts???
Questions
1) Would PWHT the vessel prevent this???
2) Could/should I specfiy the lugs be Alloy 800???
3) The lugs are attached to the vessel with a SA-285 pad. I'm thinking if I change the Pad to Alloy 800, the dissimilar weld will be moved off the pressure retaining shell.
Thoughts???