Quality2479
Materials
Hi,
Good Day Everyone
Code- ASME Sec.IX
Process - GTAW+GMAW
Type- Automatic Welding
Pipe Size & Material - Dia 6" Sch.80 (10.97mm), SA106 Gr.B
Welding Consumable used - GTAW-ER70S-2 (Shielding Argon 99.997%) and GMAW-ER70S-2 (Shielding 80%Ar+20%Co2)
GTAW Deposition-3.8mm, GMAW-7.17mm
100% RT acceptable joint.
Inspite of clearing 100% RT of PQR sample, our test sample was failed in Bend Test and found with open cracks, we are not able to make it why?, the welding consumable selection was according to the Electrode manufacturer and process selection was as per the Welding machine manufacturer, all the welding parameters were recorded and found the Maximum heat input as 1.9Kj/mm.
Can any one advice on this? so that we can goahead with some changes in Procedure Qualification.
Thanks in advance.
Good Day Everyone
Code- ASME Sec.IX
Process - GTAW+GMAW
Type- Automatic Welding
Pipe Size & Material - Dia 6" Sch.80 (10.97mm), SA106 Gr.B
Welding Consumable used - GTAW-ER70S-2 (Shielding Argon 99.997%) and GMAW-ER70S-2 (Shielding 80%Ar+20%Co2)
GTAW Deposition-3.8mm, GMAW-7.17mm
100% RT acceptable joint.
Inspite of clearing 100% RT of PQR sample, our test sample was failed in Bend Test and found with open cracks, we are not able to make it why?, the welding consumable selection was according to the Electrode manufacturer and process selection was as per the Welding machine manufacturer, all the welding parameters were recorded and found the Maximum heat input as 1.9Kj/mm.
Can any one advice on this? so that we can goahead with some changes in Procedure Qualification.
Thanks in advance.