Copper water lines are very common for industrial service. If it's relatively cold water, the lines can sweat during the summer, resulting in drips that can cause problems with other equipment or slippery floors. Insulating the lines is the usual solution.
Copper piping for compressed air service is sometimes used. In many general industrial plants, the joints are often soft soldered. I've had several inspectors tell me that this isn't strictly prohibited by code, but I wouldn't do it. These joints can fail if there's a fire in the plant, as there's no liquid in the pipe to keep them cool. If you're using copper for compressed air, have somebody licenced under Section IX silver solder the joints.