Could you share experiences to prevent welding defect type Lack of fusion on material Pipe SA335-P92 (OD 219 x T61) with Stub SA213-T92 (OD 43.2 x T9.2) ?
Now we use welding rod GTAW ER90S-G(Bohle Thermanit MTS 616) , Preheating by electric Pad keep the temperature min 205°C and interpass max 300°C