dear all,
i have approved WPS for groove of Carbon Steel comply with ASME IX code ( max. 11mm thickness). so now can i weld with double bevel with 18 mm of thickness? because of with single bevel joint i can weld two side and with each side i have imagined as single bevel of 9mm thickness. (mid of 18mm is 9mm). please correct my thinking
i have approved WPS for groove of Carbon Steel comply with ASME IX code ( max. 11mm thickness). so now can i weld with double bevel with 18 mm of thickness? because of with single bevel joint i can weld two side and with each side i have imagined as single bevel of 9mm thickness. (mid of 18mm is 9mm). please correct my thinking