Hi
We have 2 boilers 185 t/hr steam coal/bagasse with Hamon ESP. We notice lots of ash particles inside the penthouse where there are the isolating ceramic and discharge electrode hammers during annual shutdown. The ash deposit on the ceramic isolators and may cause cracking.
The penthouse is in depression as the ID fan is blowing the flue gas. So we should not expect to see ash moving up inside the penthouse. There is a heater blower fan on top of the ESP which is only used as start up of the plant. During operation, it is stopped. We have noticed there are 3 holes on the metal plate on top of the ceramic isolators with a 20 mm pipe length 100 mm going down. What is the purpose of this pipe? Can we closed the 3 holes? Plz see attached picture.
Has someone encounter this ash problem and how it was solved? Thks
We have 2 boilers 185 t/hr steam coal/bagasse with Hamon ESP. We notice lots of ash particles inside the penthouse where there are the isolating ceramic and discharge electrode hammers during annual shutdown. The ash deposit on the ceramic isolators and may cause cracking.
The penthouse is in depression as the ID fan is blowing the flue gas. So we should not expect to see ash moving up inside the penthouse. There is a heater blower fan on top of the ESP which is only used as start up of the plant. During operation, it is stopped. We have noticed there are 3 holes on the metal plate on top of the ceramic isolators with a 20 mm pipe length 100 mm going down. What is the purpose of this pipe? Can we closed the 3 holes? Plz see attached picture.
Has someone encounter this ash problem and how it was solved? Thks