Hi,
Can anyone point me to references to determine the erosion rate of steel that is being blasted by a fluid spray. I'm trying to determine how thick to make a plate that will be used to contain a leak emanating from a high temp/high pressure source. I'm trying to solve a problem such as: if a 500 degree, 500 psi system began leaking from a 0.125" hole onto a 0.375" plate (12" away); how long before the plate was punctured?
thanks,
Dave
Can anyone point me to references to determine the erosion rate of steel that is being blasted by a fluid spray. I'm trying to determine how thick to make a plate that will be used to contain a leak emanating from a high temp/high pressure source. I'm trying to solve a problem such as: if a 500 degree, 500 psi system began leaking from a 0.125" hole onto a 0.375" plate (12" away); how long before the plate was punctured?
thanks,
Dave