edine
Materials
- Aug 14, 2006
- 13
We are having matte tin plated over brass. There parts are subsequently bonded using an epoxy adhesive. This process has been working successfully for years. We are starting production at another location which means a change in plating suppliers. The last lot did not bond at all. Cleaning with isopropyl alcohol did not help, acetone did better, but not good enough. What should I be looking at in the plating process to identify the source of this type of problem? Are there any contaminants that will plate out with the tin that will cause adhesion problems? Thanks.