1
- #1
TugboatEng
Marine/Ocean
I thought this was entertaining, it's 1.5" sch 80 welded pipe as an overboard that services gray water, black water, and salt water.
That's literally the seam hanging off the bottom of the pipe.

That's literally the seam hanging off the bottom of the pipe.