Tek-Tips is the largest IT community on the Internet today!

Members share and learn making Tek-Tips Forums the best source of peer-reviewed technical information on the Internet!

  • Congratulations MintJulep on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Entertainment purposes: Don't use welded steel pipe for corrosive service, an example: 2

Status
Not open for further replies.

TugboatEng

Marine/Ocean
Joined
Nov 1, 2015
Messages
12,105
Location
US
I thought this was entertaining, it's 1.5" sch 80 welded pipe as an overboard that services gray water, black water, and salt water.

PXL_20210105_224815787_bsv4fi.jpg


That's literally the seam hanging off the bottom of the pipe.
 
At least they spent a little extra on the flange bolts [tongue]
 
I used to have a photo of a SS pipe line that had welded pipe from two suppliers.
The welds had rotted out of one, and the other was intact.

= = = = = = = = = = = = = = = = = = = =
P.E. Metallurgy, consulting work welcomed
 
This is probably continuously welded pipe. The only thing continuous about it is the name.
 
Heat treat, what heat treatment?

= = = = = = = = = = = = = = = = = = = =
P.E. Metallurgy, consulting work welcomed
 
Status
Not open for further replies.

Part and Inventory Search

Sponsor

Back
Top