GOST 380-94 is semi finished productsin carbon steel , the approx. equivalent would be A 36.
GOST 4041-71 is hot-rolled heavy plate for cold pressing
approx. equivalent A 621
At the link above, selecting the specific GOST material "Grade" (in the "Step 3" column) for either of these GOST specifications will show "Analog" specifications (scroll to the bottom of the page to see the analog specifications after clicking on the specifc grade you're interested in).