Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations 3DDave on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

EN = GOST

Status
Not open for further replies.

gyury60

Industrial
May 7, 2006
7
Hi!
Have someone a equivalent between EN si GOST please?
 
Replies continue below

Recommended for you

Say what?

Kenneth J Hueston, PEng
Principal
Sturni-Hueston Engineering Inc
Edmonton, Alberta Canada
 

Are you refeering to Global Operating Systems Technology?

Chuck
 
I have some GOST standards. Which EN standard number do you want to know the equivalent of ?
 
Dear Izer,
I want GOST 380-94,4041-71,
Thank you very much.
Your sincerely,
gyury
 
GOST 380-94 is semi finished productsin carbon steel , the approx. equivalent would be A 36.
GOST 4041-71 is hot-rolled heavy plate for cold pressing
approx. equivalent A 621
 