Hi!
Have someone a equivalent between EN si GOST please?
 
Say what?

Kenneth J Hueston, PEng
Principal
Sturni-Hueston Engineering Inc
Edmonton, Alberta Canada
 

Are you refeering to Global Operating Systems Technology?

Chuck
 
I have some GOST standards. Which EN standard number do you want to know the equivalent of ?
 
Dear Izer,
I want GOST 380-94,4041-71,
Thank you very much.
Your sincerely,
gyury
 
GOST 380-94 is semi finished productsin carbon steel , the approx. equivalent would be A 36.
GOST 4041-71 is hot-rolled heavy plate for cold pressing
approx. equivalent A 621
 
At the link above, selecting the specific GOST material "Grade" (in the "Step 3" column) for either of these GOST specifications will show "Analog" specifications (scroll to the bottom of the page to see the analog specifications after clicking on the specifc grade you're interested in).
 