Hello guys.
These slabs they are externally exposed in a soffit of a loading dock in a chopping centre, around 3km (approx 2 miles) from the Indian Ocean.
They have been in place since approx 2004 (8 Years).
Several, but not all of the units exhibit similar staining. It runs in line with direction of rebar. However no spalling is noted.
I have only visually inspected from ground level 5m (16ft)
Have a look at the image - I have a felling the rust staining is a sign of the beginning of chloride corrosion of rebar, however there is no rust staining.
These slabs they are externally exposed in a soffit of a loading dock in a chopping centre, around 3km (approx 2 miles) from the Indian Ocean.
They have been in place since approx 2004 (8 Years).
Several, but not all of the units exhibit similar staining. It runs in line with direction of rebar. However no spalling is noted.
I have only visually inspected from ground level 5m (16ft)
Have a look at the image - I have a felling the rust staining is a sign of the beginning of chloride corrosion of rebar, however there is no rust staining.