Trying to figure out the essential variable "A"# for E7010-P1. Ive compared the analysis from both the spec in sect 2 (SFA.5.5) and from a sample test report from Lincoln (pipeliner 7p+) and the analysis doesnt fit any A number on the table. The nickel(1.00max sect 2, typ 0.58-0.90 from the mfr)
What am I missing?