E7010-P1 A number ASME IX Table QW-442

Status
Not open for further replies.

rmillercwi

Materials
Joined
Jul 19, 2006
Messages
76
Location
US
Trying to figure out the essential variable "A"# for E7010-P1. Ive compared the analysis from both the spec in sect 2 (SFA.5.5) and from a sample test report from Lincoln (pipeliner 7p+) and the analysis doesnt fit any A number on the table. The nickel(1.00max sect 2, typ 0.58-0.90 from the mfr)

What am I missing?
 
I don't think you are missing anything. Not all weld deposits will fit in a A number. QW-404.5 has alternatives.
 