Sep 8, 2011 #1 MSSandvik Materials Joined May 24, 2010 Messages 9 Location SE Does anyone know if there are any standard drill point geometries for CFRP drilling? By this i mean NAS 907 describes some drills and the metals they're to be used on. Is there one for CFRP? Any help appreciated
Does anyone know if there are any standard drill point geometries for CFRP drilling? By this i mean NAS 907 describes some drills and the metals they're to be used on. Is there one for CFRP? Any help appreciated
Sep 8, 2011 #2 rerig Aerospace Joined Aug 6, 2003 Messages 286 Location US Page 19 http://files.engineering.com/getfile.aspx?folder=9f5458f5-3677-4785-9d3c-85facb373ed2&file=6M62-656_Machining_Plastics_and_Advanced_Composites.pdf Upvote 0 Downvote
Sep 9, 2011 Thread starter #3 MSSandvik Materials Joined May 24, 2010 Messages 9 Location SE rerig Nice one, this looks good. I assume the ST10-907-A is a NAS 907 A point geomtery? Thanks for your help. Upvote 0 Downvote
rerig Nice one, this looks good. I assume the ST10-907-A is a NAS 907 A point geomtery? Thanks for your help.