One of the components in our product is of Carbon Fibre-Sandwich construction.

We have to get NDT done on our initial parts. Before carrying out NDT, we need to characterise the defects by training the machine. Are there any open-source guidelines available on introducing different types of defects, sizes of the defects & their locations?
 
For starters???

FAA AC43-214 Repairs and Alterations to Composite and Bonded Aircraft Structure

ASTM E2533 Standard Guide for Nondestructive Examination of Polymer Matrix Composites Used in Aerospace Applications

ASTM E3370 Standard Practice for Matrix Array Ultrasonic Testing of Composites, Sandwich Core Constructions, and Metals

AIA/NAS NAS999 [cx] NONDESTRUCTIVE INSPECTION OF ADVANCED COMPOSITE STRUCTURES

SAE AIR4844 Composites and Metal Bonding Glossary

SAE AIR5719 Teaching Points for an Awareness Class on "Critical Issues in Composite Maintenance and Repair"

SAE ARP1611 Quality Inspection Procedure, Composites Tracer Fluoroscopy and Radiography

SAE ARP5089 COMPOSITE REPAIR NDT/NDI HANDBOOK

SAE ARP5605 Solid Composite Laminate NDI Reference Standards

SAE ARP5606 Composite Honeycomb NDI Reference Standards

MIL-HDBK-731 NONDESTRUCTIVE TESTING METHODS OF COMPOSITE MATERIALS - THERMOGRAPHY

MIL-HDBK-732 NONDESTRUCTIVE TESTING METHODS OF COMPOSITE MATERIALS ACOUSTIC EMISSION

MIL-HDBK-733 NONDESTRUCTIVE TESTING METHODS OF COMPOSITE MATERIALS - RADIOGRAPHY

MIL-HDBK-787 NONDESTRUCTIVE TESTING METHODS OF COMPOSITE MATERIALS-ULTRASONIC

MIL-HDBK-793 NONDESTRUCTIVE TESTING TECHNIQUES FOR STRUCTURAL COMPOSITES

MIL-HDBK-333-V1 & -V2 HANDBOOK FOR STANDARDIZATION OF NONDESTRUCTIVE TESTING METHODS

MIL-HDBK-337 ADHESIVE BONDED AEROSPACE STRUCTURE REPAIR

SAE R-336 Care and Repair of Advanced Composites

And if You can find it...

USAF T.O. 1-1-690 General Advanced Composite Repair Processes Manual

etc... etc...

Regards, Wil Taylor
o Trust - But Verify!
o For those who believe, no proof is required; for those who cannot believe, no proof is possible. [variation, Stuart Chase]
o Unfortunately, in science what You 'believe' is irrelevant. ["Orion", HBA forum]
o Only fools and charlatans know everything and understand everything." -Anton Chekhov
 
B2K... are your still with us?

Regards, Wil Taylor
o Trust - But Verify!
o For those who believe, no proof is required; for those who cannot believe, no proof is possible. [variation, Stuart Chase]
o Unfortunately, in science what You 'believe' is irrelevant. ["Orion", HBA forum]
o Only fools and charlatans know everything and understand everything." -Anton Chekhov
 
Status
Not open for further replies.

Part and Inventory Search

Sponsor

Back
Top