Any body can tell me the difference between Satin Coat and Galvanized Sheet? Thanks.
 
Replies continue below

Recommended for you

I know what galvanized sheet is - but not "satin coat". Galvanized sheet is steel sheet that is zinc plated. Satin coat sounds like a texture, possibly of a zinc plating, but more likely a paint.
 