hello,

any material available on difference between gmaw stt and pusle mode of metal transfer and also how select or decide mode of metal transfer in gmaw.
 
Replies continue below

Recommended for you

STT is considered short circuiting transfer, albeit with a controlled wave form; it does not produce spray transfer during a high energy pulse and does not have a background (low energy) pulse as does pulsed transfer.
 