Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations waross on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Diff. Between SA 387 Gr.11 CL1 and Cl.2 material

Status
Not open for further replies.

vinstein

Mechanical
Apr 19, 2011
10
HI all,

Can anyone tell me the difference between SA 387 Gr.11 CL1 and Cl.2 material and their usage in pressure vessel design
 
Replies continue below

Recommended for you

Class 2 plates will have a higher minimum tensile and yield than the Class 1 plates. If you can get a copy of the SA-387 spec, you will see.

I believe that the Class 2 plates will therefore have higher stress values that can be used in the design calculations. This can be verified in Section II, Part D, I don't have a copy of that handy.
 
Yes, higher allowable stress values apply for Class 2.
 