How to measure the DFT of MIO coatings?

We know MIO is magnetic, and it may affect the reading of a magnetic DFT gauge. In this case, how we can measure the DFT (Non destrutive) ?

Regards

Cococa
 
ASTM D6312

Fischer Technology seem fairly adamant that MIO doesn't affect their FMP magnetic instruments.

Steve Jones
Corrosion Management Consultant


All answers are personal opinions only and are in no way connected with any employer.
 
Thanks for your prompt reply.

But what does this ASTM D6312 for? Anything related to my query? Was it a typo?

Regards

Cococa
 
Ah yes - I see the confusion. Typo: it's D6132[blush]. You can still look it up though[glasses]

Steve Jones
Corrosion Management Consultant


All answers are personal opinions only and are in no way connected with any employer.
 
Try this....non-magnetic. Works on a variety of substrates....

Positector
 
Thank you for your interest and reply.

But, please check again. It is a magnetic probe for ferrous substrates !

Thanks

Cococa

 
Cococa,

The Positector 6000 uses both magnetic AND eddy current sensors so that it can be use on all metals.
 