Feb 12, 2003 #1 PrImpEng Automotive Joined Oct 10, 2002 Messages 3 Location GB We have a partial specification of cast iron BLS21??? and are trying to establish the density of the material for dynamic balance correction purposes.
We have a partial specification of cast iron BLS21??? and are trying to establish the density of the material for dynamic balance correction purposes.
Feb 13, 2003 #2 IanIV Mechanical Joined Feb 10, 2003 Messages 4 Location AU Is it nor 7450kg /cubic metre ? Upvote 0 Downvote
Mar 7, 2003 #3 rbigge Materials Joined Mar 7, 2003 Messages 2 Location US Density of Iron (#/in3)= 517-13.95*%C -5.67*%Si-4.43*%P This formula is per H.T. Angus published in his book "Cast Irons Physical and Engineering Properties" Upvote 0 Downvote
Density of Iron (#/in3)= 517-13.95*%C -5.67*%Si-4.43*%P This formula is per H.T. Angus published in his book "Cast Irons Physical and Engineering Properties"
Mar 17, 2003 #4 sbi Industrial Joined Sep 25, 2000 Messages 103 Location US here is the old fashion english version 0.256 LB per cubic inch ave. Upvote 0 Downvote
Jan 3, 2004 #5 crrchina Industrial Joined Jan 3, 2004 Messages 1 Location CN Please advise the comparisons between BSEN 275 J2G3 and BSEN 275 JR. Thanks. Upvote 0 Downvote