Hi,
I want to know what is DELTA sheet steel, if someone knows.
Thank you very much,
Gyury
 
Replies continue below

Recommended for you

Comeback with a little more information.
Are you referring to plain steel or a corrosion resistant material?
Are you referring to material less than 6 mm?
 
hi! I'm back,
Someone want steel sheet DELTA 30x2000x6000 S 235 JRG2, but I heare nothing about this quality DELTA.
Thank you for your time.
Gyury
 
Hi!
I know what is S 235 JRG2 but I want to know what is DELTA.
Ok! Tks anyway!
 
I searched different combinations of Delta S235 JRG2 and had numerous hits with the "Delta" in the text though the site itself was in different European languages. I saw a lot of hit with Checkoslovakian (cz) addresses. Several also mentioned galvanizing with S235 JRG2.
 
is DELTA a steel producer or service center.. often the guy making the print doesnt know how the sheet steel industry is setup.

(Example: one of our customers requires we buy steel from a particular service center, it doesnt matter who manufactured the steel or who rolled it, just who slit it.)

Nick
I love materials science!
 
Thank you all!You are very kind.
Gyury
 