Does it safe to cleaning electrical parts/panel using Deionization Water?
 
You may need to check how clean your DI water is.
You are usually talking about water with a resistivity of >18Mohm-cm.
And it also should have control for biological activity, dissolved gases, and many trace elements.
Even very small amounts of residuals can harm electronics.
True high purity water will have less than 100ng/l of residue.
 
Ultrapure water, exposed to air, is actually a bit acidic due to dissolving CO2

However, we typically do not use water, since moisture can lead to corrosion. See this and that for alternative. Note that even when we do use water for cleaning, we use IPA as the final rinse, since it tends to take away the water more thoroughly.
 