Jun 5, 2001 #1 carolina8 Chemical Joined May 18, 2001 Messages 5 Location MX hi everyone: i want to meassure the degree of a dispersion of a solid in water by some instrument in the plant and by some analitical tech in the lab.
hi everyone: i want to meassure the degree of a dispersion of a solid in water by some instrument in the plant and by some analitical tech in the lab.
Jun 12, 2001 #2 implant Materials Joined Mar 12, 2007 Messages 2 Location JP For a quick fineness of grind the Hegman gauge could be used in the plant while for paricle size distribution a laser particle size analyzer and optical microscope would help Upvote 0 Downvote
For a quick fineness of grind the Hegman gauge could be used in the plant while for paricle size distribution a laser particle size analyzer and optical microscope would help