CompositeGeek
Aerospace
Okay - I am out of my professional depth but here goes:
1. What (if any) advantage does cryo treatment of common aerospace titanium alloys provide? Wear resistance? Fatigue life iprovement? Property characteristics?
2. How is the treatment impacted by alloy of titanium? 6AL-4V vs 5-5-5-3 as an example.
3. I know certain steels benefit, and according to Golf Digest Titanium clubs are helped(still looking at this) But how about Inconel? Any benefits?
4. If Cryo treatment improves wear resistance in steel but then the part is shotpeened after treatment does that have a negative impact on the level of benefit?
Thanks in advance. Any feedback is appreciated!!!
Composites and Airplanes - what was I thinking?
There are gremlins in the autoclave!
1. What (if any) advantage does cryo treatment of common aerospace titanium alloys provide? Wear resistance? Fatigue life iprovement? Property characteristics?
2. How is the treatment impacted by alloy of titanium? 6AL-4V vs 5-5-5-3 as an example.
3. I know certain steels benefit, and according to Golf Digest Titanium clubs are helped(still looking at this) But how about Inconel? Any benefits?
4. If Cryo treatment improves wear resistance in steel but then the part is shotpeened after treatment does that have a negative impact on the level of benefit?
Thanks in advance. Any feedback is appreciated!!!
Composites and Airplanes - what was I thinking?
There are gremlins in the autoclave!