Roker,
It certainly depends on crude corrosivity, i.e. salts, water, naphthenic acid, H2S and other aggressive agents. Cladding is - as far as I know - very acceptable and effective approach. But I would definitely suggest you to consult experienced corrosion engineers and to examine the worst possible scenario regarding feed quality and corrosion mechanisms that may occur.
Regards,