Elnur250774
Materials
Hello there,
I've been told by supplier that "For Quality S235 it is always issued MTC 2.2, which does not provide indication of Heat Number" Is it right?
As per EN 10204 clause 3.2: Test report "type 2.2"
Document in which the manufacturer declared that the products supplied are in complience with the requirements of the order and in which the supplier test results based on non-specific inspection.
1.Why it is always 2.2 cert?
2.So how I can be sure that test results belongs to exactly that heat numbered material?
3.What actually stated in 2.2 certificate?
I've been told by supplier that "For Quality S235 it is always issued MTC 2.2, which does not provide indication of Heat Number" Is it right?
As per EN 10204 clause 3.2: Test report "type 2.2"
Document in which the manufacturer declared that the products supplied are in complience with the requirements of the order and in which the supplier test results based on non-specific inspection.
1.Why it is always 2.2 cert?
2.So how I can be sure that test results belongs to exactly that heat numbered material?
3.What actually stated in 2.2 certificate?