In looking at ACI318-02, I am a bit confused with regards to an item shown in the flowchart of Figure R5.3.
The item reads:
"Field record of at least ten consecutive test results using similar materials and under similar conditions is available"
This seems odd to me.
Isn't the point of allowing a concrete facility the use of the field experience approach to give them a method that permits them to utilize their past record as long as those records are based on "similar materials and under similar conditions"? The way I read this item, it says only ten of them need to meet this criteria. What about the other five to twenty tests (based on 15 to 30 total)?
What am I missing here, folks?
Thanks in advance for any insight you can offer.
The item reads:
"Field record of at least ten consecutive test results using similar materials and under similar conditions is available"
This seems odd to me.
Isn't the point of allowing a concrete facility the use of the field experience approach to give them a method that permits them to utilize their past record as long as those records are based on "similar materials and under similar conditions"? The way I read this item, it says only ten of them need to meet this criteria. What about the other five to twenty tests (based on 15 to 30 total)?
What am I missing here, folks?
Thanks in advance for any insight you can offer.