JoeBaseplate
Structural
- May 31, 2011
- 204
Party pavilion, open 4 sides, wood trusses on columns at roof. Location in IL (frost and snow). My question is about my slab on grade mix design. I have the following:
Min f’c = 3000 psi.
Min cement. Material = 520 lb/cubic yd.
Max W/C = 0.40
Slupm = 4” + - 1”
Air content = 5.5% + - 1
This is the typical SOG design we use for interior slabs. Should I change anything for the exterior use?
Min f’c = 3000 psi.
Min cement. Material = 520 lb/cubic yd.
Max W/C = 0.40
Slupm = 4” + - 1”
Air content = 5.5% + - 1
This is the typical SOG design we use for interior slabs. Should I change anything for the exterior use?