rowingengineer
Structural
I have a few questions so please bear with me if you have the time. I am not expert in mix design, normally just specifying standard mix’s ie N40 or N32. am before you think i am over stepping the mark, I will be getting My mix design reviewed and tested by the concrete supplier however I need to have something that is +/- 20% for costing purposes.
I have two buildings to design, one is a tank for the storage of wastewater and the other is a heating airbox.
The waste water has a PH of 5.5, So I am thinking that i will need some Silica fume and will use siliceous Agg.
My Mix design is S40, 330kg/m3 of cement, 50kg/m3 of silica fume and w/c of 0.4. 20mm agg
Does this sound ok, and what type of aggregate would be siliceous?
For the heating air box, I have a building that will be heated to 95deg then cooled rather quickly in 12hr cycles.
I would like to densify the concrete thus am thinking of 30kg/m3 silica fume, 420kg/m3 of cement w/c 0.3. I am also considing using some fly ash as replacement for cement. 20mm agg.
Soes this sounds ok? Does fly ass help and what replacement would you use, say 350kg/m3 cement with 70kg/m3 flyash?
Any thoughts wuld be appricated, as the closer i get now the better the costing and testing.
When in doubt, just take the next small step.
I have two buildings to design, one is a tank for the storage of wastewater and the other is a heating airbox.
The waste water has a PH of 5.5, So I am thinking that i will need some Silica fume and will use siliceous Agg.
My Mix design is S40, 330kg/m3 of cement, 50kg/m3 of silica fume and w/c of 0.4. 20mm agg
Does this sound ok, and what type of aggregate would be siliceous?
For the heating air box, I have a building that will be heated to 95deg then cooled rather quickly in 12hr cycles.
I would like to densify the concrete thus am thinking of 30kg/m3 silica fume, 420kg/m3 of cement w/c 0.3. I am also considing using some fly ash as replacement for cement. 20mm agg.
Soes this sounds ok? Does fly ass help and what replacement would you use, say 350kg/m3 cement with 70kg/m3 flyash?
Any thoughts wuld be appricated, as the closer i get now the better the costing and testing.