azonicbruce
Mechanical
Just thought I'd give an update on what was going on. Here's the original thread that you can refer to:
thread507-86835
Well, after dumping more than 1000 cubic yards of dirt, the pad fill is pretty much done. I'm not sure what type of dirt was used, but it pretty much seemed like the same dusty, loose type of dirt that is oh-so-abundant in El Paso. See the pics below.
I have a copy of the Nuclear Density Test. Here are the numbers:
Location 1:
Wet Dens.- 128.6
%Moist.- 11.1
Dry Dens.- 115.8
%Comp.- 100.7
Opt Moist.- 11.5
Max Dens.- 115.0
Probe Depth- 12"
Location 2:
Wet Dens.- 128.1
%Moist.- 11.9
Dry Dens.- 114.4
%Comp.- 99.4
Opt Moist.- 11.5
Max Dens.- 115.0
Probe Depth- 12"
Location 3:
Wet Dens.- 127.6
%Moist.- 13.3
Dry Dens.- 112.6
%Comp.- 97.9
Opt Moist.- 11.5
Max Dens.- 115.0
Probe Depth- 12"
Quick question. 100.7% Compaction? Is that even possible?
Anyway I'm wondering if these numbers seem to jive, considering the type of dirt used. I should have pictures of the final fill sometime soon.
thread507-86835
Well, after dumping more than 1000 cubic yards of dirt, the pad fill is pretty much done. I'm not sure what type of dirt was used, but it pretty much seemed like the same dusty, loose type of dirt that is oh-so-abundant in El Paso. See the pics below.
I have a copy of the Nuclear Density Test. Here are the numbers:
Location 1:
Wet Dens.- 128.6
%Moist.- 11.1
Dry Dens.- 115.8
%Comp.- 100.7
Opt Moist.- 11.5
Max Dens.- 115.0
Probe Depth- 12"
Location 2:
Wet Dens.- 128.1
%Moist.- 11.9
Dry Dens.- 114.4
%Comp.- 99.4
Opt Moist.- 11.5
Max Dens.- 115.0
Probe Depth- 12"
Location 3:
Wet Dens.- 127.6
%Moist.- 13.3
Dry Dens.- 112.6
%Comp.- 97.9
Opt Moist.- 11.5
Max Dens.- 115.0
Probe Depth- 12"
Quick question. 100.7% Compaction? Is that even possible?
Anyway I'm wondering if these numbers seem to jive, considering the type of dirt used. I should have pictures of the final fill sometime soon.