Is it just residue on the surface? Was this surface previously in contact with the subgrade and is that subgrade that color?

Otherwise, when you chip away at that blue-gray surface do you find more blue-gray beneath?

Check out Eng-Tips Forum's Policies here:
faq731-376
 
Yes.... likely slag cement mixed with portland cement. Commonly done.

Gives a blue-gray color that will change to gray upon long term exposure to air. Not a concern unless there are other issues.

You can see in the photo that the upper part of the section has already oxidized and at a point below where the section was in contact with the ground, the change has not yet occurred.
 