Compress forcing normalization of flange in Appx 1-6

Status
Not open for further replies.

BigTank

Mechanical
Joined
Sep 24, 2007
Messages
368
Location
US
I'm designing a dished cover with a bolting flange like Fig. 1-6 sketch D (Appendix 1-6). I cannot find in the code where SA-516 Gr. 70 material used for the flange must be normalized (at 3-1/4 thick), but Compress keeps forcing it.

Please help me find this in the code! It's driving me CRAZY!

--------------------------------
Fitter, happier, more productive
 
i think that any plate that thick requires normalizing for asme code
 
BigTank,

It is in the material spec. for SA-516...Section 5.2 which says,

"Plates over 1.50 in. [40 mm] in thickness shall be normalized."
 
thanks doct...i was just logging in to post that i found that information myself.

man, sometimes chasing stuff down can be frustrating!

thanks, gents!

--------------------------------