Jan 9, 2013 1 #1 ozzy1 Mechanical Joined Feb 9, 2011 Messages 30 Location US We are trying to get a hardness comparison between Chinese 303, 304, US 416 and FN-0205-25. Any help wouls be greatly appreciated
We are trying to get a hardness comparison between Chinese 303, 304, US 416 and FN-0205-25. Any help wouls be greatly appreciated
Jan 9, 2013 1 #2 TVP Materials Joined Apr 12, 2002 Messages 4,592 Location US 303 --> 83 to 87 HRB 304 --> 70 to 80 HRB 416 --> 82 to 87 HRB FN 0205 --> 59 to 65 HRB Upvote 0 Downvote