We are trying to get a hardness comparison between Chinese 303, 304, US 416 and FN-0205-25. Any help wouls be greatly appreciated
 
Replies continue below

Recommended for you

303 --> 83 to 87 HRB
304 --> 70 to 80 HRB
416 --> 82 to 87 HRB
FN 0205 --> 59 to 65 HRB
 