If I am making a wide flange beam to column connection and I provided a CJP weld at the flanges to develop moment, am I allowed to provided a bolted web plate connection as well to take the shear force?
I remember reading somewhere that you can't do that, because you may have to fail the welds in flanges to engage the bolts in shear at web.