struct_eeyore
Structural
I have a number of columns that are exhibiting spalling immediately below bearing. As far as we can tell, these are superficial and don't progress beyond reinforcement. The beams above have not yet been loaded yet. The spalls occur on random sides of the columns along any one grid line. Other than improper spacing and cover of ties, what could be the cause? Some of the columns also have horizontal (possibly shrinkage?) cracks, which I've never seen.
edit: title