Jun 1, 2021 #1 ellas1 Structural Joined Dec 20, 2011 Messages 28 Location US What is the Cold & Hot Allowable Stress for A778 304L pipe. I cannot find this material on B31 tables. Thank you
What is the Cold & Hot Allowable Stress for A778 304L pipe. I cannot find this material on B31 tables. Thank you
Jun 1, 2021 #2 XL83NL Mechanical Joined Mar 3, 2011 Messages 3,120 Location NL Which B31 code section do you require? Huub - You never get what you expect, you only get what you inspect. Upvote 0 Downvote
Which B31 code section do you require? Huub - You never get what you expect, you only get what you inspect.
Jun 1, 2021 Thread starter #3 ellas1 Structural Joined Dec 20, 2011 Messages 28 Location US I am not looking for B31 code. I am looking for the allowable stress for this material because it is not listed on B31. Th elates t I have is 2018. Thank you Upvote 0 Downvote
I am not looking for B31 code. I am looking for the allowable stress for this material because it is not listed on B31. Th elates t I have is 2018. Thank you
Jun 1, 2021 1 #4 GD2 Mechanical Joined Sep 25, 2017 Messages 729 Location CA Ellas1, What is the hot/design temperature? GDD Canada Upvote 0 Downvote
Jun 1, 2021 1 #5 XL83NL Mechanical Joined Mar 3, 2011 Messages 3,120 Location NL B31.1, B31.3, B31.?? It will determine whether and how you might an unlisted material. Huub - You never get what you expect, you only get what you inspect. Upvote 0 Downvote
B31.1, B31.3, B31.?? It will determine whether and how you might an unlisted material. Huub - You never get what you expect, you only get what you inspect.
Jun 1, 2021 1 #6 EdStainless Materials Joined May 20, 2004 Messages 16,366 Location Waukesha WI USA I don't believe that you can use A778 because it is unannealed product. = = = = = = = = = = = = = = = = = = = = P.E. Metallurgy, consulting work welcomed Upvote 0 Downvote
I don't believe that you can use A778 because it is unannealed product. = = = = = = = = = = = = = = = = = = = = P.E. Metallurgy, consulting work welcomed