Location
GB
I want to know if there is a clear plastic tube that is suitable for exposure to 160degsC. The ID needs to be 4" but the wall thickness is not important.

It forms part of a test rig but will be backed up with a steel casing with slots so that we can see in.

Would glass be an option - just thinking about it (and looking out of the window!)

Cheers

Phil.
 
How clear, any load or chemicals in the environment.

Off the top of my head, TPX might take 160, polycarbonate probably won't, Polysulphone will. Amorphous nylons probably will.

I don't expect any except the polycarbonate are available ex stock, but if the requirement was sufficient, they could all be made.

Regards
pat pprimmer@acay.com.au
eng-tips, by professional engineers for professional engineers
Please see FAQ731-376 for tips on how to make the best use of Eng-Tips Fora.
 
One big supplier of ex stock tubes and profiles made of various engineering and high-temperature plastics is a company called Ensinger. Check them out at I'm sure they have what you need.
 
The temperature is going to be the tough one. I would suggest tempered glass as the material.
 