Hello Everyone,
After installing the clean out and due to wrong welding process, the contractor had to cut and reweld the clean out neck again. Is this permissible in API 650. I would appreciate if someone can refer us to a clause in API that cover this type of issues.
Thank you
Hello Everyone,
After installing the clean out and due to wrong welding process, the contractor had to cut and reweld the clean out neck again. Is this permissible in API 650. I would appreciate if someone can refer us to a clause in API that cover this type of issues.