Yesterday at 6:41 PM #1 GOSP75 Mechanical Joined Feb 27, 2016 Messages 8 Location QA We have API 650 stainless steel storage tanks of 3m and 4m dia bottom plate having butt weld configuration without back strip. The weld joints on soil side required Pickling and passivation?. Soil side no painting. Regards, Shanmuga