Deformation on API 650 tank bottom

Status
Not open for further replies.

tankinspector88

Mechanical
Jun 7, 2024
13
How can I evaluate if I need to replace a deformed bottom plate?
Its a 12m long carbon steel plate and in some points MFL stucked because the deformation.
 
Replies continue below

Recommended for you

API-653 has procedures to determine if a localized low spot in a bottom needs to be repaired.
 