Hi,
I was hoping to get some help here.
A class 300 nipple (2 in sched. 80) I chose for my design (Class 300), is capable of holding 1500 psig of pressure from (-29 to 66 Celsius). However when I calculate this nipple as per B31.3 having into account: 12.5% under tolerance allowance, 0.118 Corrosion Allowance (sea water), and h=.06597 in thread depth I just don't meet the minimum thickness required.
What do you usually do in this situation?
JJAV1983
I was hoping to get some help here.
A class 300 nipple (2 in sched. 80) I chose for my design (Class 300), is capable of holding 1500 psig of pressure from (-29 to 66 Celsius). However when I calculate this nipple as per B31.3 having into account: 12.5% under tolerance allowance, 0.118 Corrosion Allowance (sea water), and h=.06597 in thread depth I just don't meet the minimum thickness required.
What do you usually do in this situation?
JJAV1983