Dear All,
I am in a situation wherein there is a 2" SS Drain piping to be supported by CS bolted clamped shoe.
There are no insulators like liners etc. to avoid the contact in between the 2 different metals CS with SS.
Kindly advice on this at the earliest about how this is done or the above situation is acceptable?
What are the various ways to avoid the SS to CS contact in above situation?
Thanks & Regards,
Abhijit
Dear All,
I am in a situation wherein there is a 2" SS Drain piping to be supported by CS bolted clamped shoe.
There are no insulators like liners etc. to avoid the contact in between the 2 different metals CS with SS.
Kindly advice on this at the earliest about how this is done or the above situation is acceptable?
What are the various ways to avoid the SS to CS contact in above situation?
Thanks & Regards,