Sep 26, 2007 #1 laxboy4788 Materials Joined Sep 26, 2007 Messages 3 Location US I am wondering which material, Zinc Die Cast or Aluminum Die Cast, Chrome Plating would bound and adapt to better. Say if the part is going to be used in an outdoor grill.
I am wondering which material, Zinc Die Cast or Aluminum Die Cast, Chrome Plating would bound and adapt to better. Say if the part is going to be used in an outdoor grill.
Sep 26, 2007 #2 swall Materials Joined Sep 30, 2003 Messages 2,767 Location US Both can be satisfactorily chrome plated for outdoor decorative applications. Upvote 0 Downvote
Sep 26, 2007 #3 lgearhart Materials Joined Jan 31, 2002 Messages 66 Location US You're going to keep that zinc die cast part away from the hot part of the grill, right? Upvote 0 Downvote
Sep 27, 2007 Thread starter #4 laxboy4788 Materials Joined Sep 26, 2007 Messages 3 Location US the part would be on the outside of the grill say like where a company's logo would be Upvote 0 Downvote
Sep 27, 2007 Thread starter #5 laxboy4788 Materials Joined Sep 26, 2007 Messages 3 Location US my real question is which of those materials would bond to chrome plating better, in general Upvote 0 Downvote
Sep 28, 2007 #6 kenvlach Materials Joined Apr 12, 2000 Messages 2,514 Location US Zinc alloy is easier to plate and costs less to die cast (lower melting temperature) than aluminum alloy. See FAQ about Die Casting http://www.diecasting.org/faq/#Proper Upvote 0 Downvote
Zinc alloy is easier to plate and costs less to die cast (lower melting temperature) than aluminum alloy. See FAQ about Die Casting http://www.diecasting.org/faq/#Proper