I am designing a tool that will go into a heat furnace at 850F degrees for 30 minutes, and need to decide what grade steel to make the tool out of. I was originally thinking 304 or 316SS due to its high temperature properties, but cost is significantly more than A36 or a low carbon steel. Trying to determine what grade, or ASTM spec of steel would work for this application? Note, structurally this tool will not be withstanding high loads. Thanks all..