1
I previously worked on project were the bridge piers of a highway passing over a major dual carriageway had been attacked by chloride. The road was subject to sub-zero conditions and a chlorine based de-icier was used to stop the road from freezing. The sub-grade of the road was slag, a by product of burning coal in power stations with good engineering properties. But the combination of the slag and the chloride attacked the concrete to the piers rapidly and cause the concrete to become extremely weak. I think the process or chemical reaction is called Thauximite. But I need conformation on this and also what was the chemical reaction between the slag, chlorine and concrete. Thanks is advance for any suggestions.
 
Replies continue below

Recommended for you

Hello Rich,

It sounds a little like thaumasite sulfate attack. The samples of it that I have sitting on my desk (I am a very sad person) show bands of white through the concrete and are easily damaged by fingernails.

I have only had a brief contact with this sort of problem but WS Atkins (Britain), maintaining agents for the Highways Agency Area 2 (near Bristol) have a lot of experience regarding this subject. There has been several conferences and and papers on this problem but I confess I can't give you any guide here.
 
RichinEthiopia,

You might consult


This is the website of the Building Research Establishment in the UK. Follow the links to Concrete or the links to the BRE Bookshop.

Similarly


is the website of the UK Transport Research Laboratory from which I copied the following publication details. You should visit the website yourself to obtain a more suitable search result.

The influence of chlorides on the alkalinity of concrete
Report No. LR 915
Author(s): P R Vassie. 1979
Price: £20.00

An international review of chloride ingress into structural concrete. 1997
Report No. CR359/BR
Author(s): P B Bamforth, W F Price, M Emerson
Price: £30.00

Methods to determine chloride concentrations in in-situ concrete. 1986
Report No. CR32
Author(s): J W Figg
Price: £20.00
 