We have 6 concrete cooling towers (wet/dry cycles are common) that are fast deteriorating by spalling. We suspect that chert was used in the aggregate and that it is causing chunks to pop at the surface. I need information on the behavior and composition of chert. The chert near the surfaces are poping now, but how about the chert that is deep in the wall? (12 thick and thicker) is that chert also deteriorating inside?. How is best to repair? Can a waterprofing coat with a high-tech material help? or retard deterioration of the cooling towers. The are about 5-years old. Your insights will be appreciatted